Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Cumar P10 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 149 °C |
0.117 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 7.00 min @Temperature 149 °C |
0.117 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 5.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 7.02 - 12.0 min | 0.117 - 0.200 hour | Tack-free time |
Master Bond MasterSil 710 Silicone Paste Meets MIL Spec Description: MasterSil 710 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This product meets the Meets MIL-.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Cumar P10 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Cure Time | 7.00 min @Temperature 83.3 °C |
0.117 hour @Temperature 182 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 83.3 °C |
0.117 hour @Temperature 182 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Vul-Cup 40KE Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min | 0.117 hour | |
Loctite® 246 High Temperature/Medium Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 149 °C |
0.117 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 7.00 min @Temperature 149 °C |
0.117 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 15.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 7.00 min | 0.117 hour | t`50, Target; ASTM D2084 |
ExxonMobil Exxon™ 2211 Fast Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber balesInformation provided by ExxonMobil Chemical |
|||
Cure Time | 7.00 min | 0.117 hour | t`50, Target; ASTM D2084 |
ExxonMobil Exxon™ 2235 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Cure Time | 7.00 min @Temperature 83.3 °C |
0.117 hour @Temperature 182 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 83.3 °C |
0.117 hour @Temperature 182 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Vul-Cup 40KE Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 160 °C |
0.117 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 7.00 min @Temperature 149 °C |
0.117 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 5.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 7.00 min @Temperature 155 °C |
0.117 hour @Temperature 311 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 7.00 min @Temperature 149 °C |
0.117 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 7.00 min @Temperature 160 °C |
0.117 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 7.00 - 10.0 min @Temperature 25.0 °C |
0.117 - 0.167 hour @Temperature 77.0 °F |
demold time |
BCC Products BC 8086 Urethane Casting BC 8086 is a rapid setting, low viscosity, polyurethane casting system. It exhibits a working life of 45 seconds and obtains a demoldable hardness at 7 - 10 minutes. Some of the features include: no.. |