Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 301 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | On Steel (Fixture) |
ND Industries 306 Surface Insensitive Instant Superglue Low viscosity for difficult to bond rubber compounds |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 333 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 325 Low-Medium Viscosity - General purposeMeets military spec Mil-A-46050C Type II Class I |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 395 General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Buna N Rubber, handling time |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Neoprene, handling time |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6010 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6011 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 43 |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 44 |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6602 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6702 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6809 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6813 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.250 min | 0.00417 hour | Steel, set time |
Permabond 200 Cyanoacrylate, wire tacking PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Cure Time | 0.250 min | 0.00417 hour | Buna N Rubber, set time |
Permabond 200 Cyanoacrylate, wire tacking PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Buna N Rubber, handling time |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Phenolic, handling time |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Cure Time | <= 0.250 min | <= 0.00417 hour | NBR Rubber, handling time |
Permabond 919 Cyanoacrylate, High temperature Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6810 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6812 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.250 - 0.417 min | 0.00417 - 0.00694 hour | Metal set time |
Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® 412 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Cure Time | 0.250 - 1.00 min | 0.00417 - 0.0167 hour | |
3M Scotch-Weld™ CA5 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity, slower setting version of CA4 for filling gaps. Meets CID A-A-3097, Type II, Clas.. |
|||
Cure Time | 0.250 min | 0.00417 hour | Set Time |
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | Time to Handling Strength |
3M Scotch-Weld™ HT700 High Temperature Instant Adhesive 3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT700 is a me.. |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | Time to Handling Strength |
3M Scotch-Weld™ MC5 Metal Instant Adhesive 3M™ Scotch-Weld™ Metal Instant Adhesives are designed to give optimum performance and high strength bonds on metals, including galvanized or anodized surfaces. MC5 (formerly SP93) is a very low vi.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Fixture Rate |
Dymax Magnet Bonder™ 2000 Adhesive DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2000 Magnet Bonder™ AdhesiveFastest cure; bond ferrite to steel. Typical Use: Loudspeaker magnet to pole piece. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® PRISM® 401 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |