Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.167 - 0.250 min | 0.00278 - 0.00417 hour | Buna N Rubber, handling time |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Cure Time | >= 0.167 min | >= 0.00278 hour | Fixture |
Resinlab® CYNERGY CA6003 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.167 min | >= 0.00278 hour | Fixture |
Resinlab® CYNERGY CA6005 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.167 min | >= 0.00278 hour | Fixture |
Resinlab® CYNERGY CA6006 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.167 min | >= 0.00278 hour | Fixture |
Resinlab® CYNERGY CA6104 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Cure Time | 0.167 - 0.500 min | 0.00278 - 0.00833 hour | zinc, Fixture time |
Permabond TA4592 Toughened Acrylic Adhesive PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt.. |
|||
Cure Time | <= 0.167 min | <= 0.00278 hour | PET, fixture time, (low power 4mW lamp) |
Permabond UV648 UV-curable Adhesive PERMABOND UV648 is a UV-curing adhesive developed for use on plastics. It has good adhesion to acrylic and contains a long-wavelength photo initiator to allow it to cure through UV-stabilized plasti.. |
|||
Cure Time | 0.167 - 0.250 min | 0.00278 - 0.00417 hour | Phenolic, handling time |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Cure Time | 0.167 - 0.250 min | 0.00278 - 0.00417 hour | Buna N Rubber, handling time |
Permabond 820 Cyanoacrylate, High Temperature PERMABOND® 820 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Cure Time | 0.167 - 0.250 min | 0.00278 - 0.00417 hour | Phenolic, handling time |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Phenolic, set time |
Permabond 931 Cyanoacrylate PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Phenolic, set time |
Permabond 935 Cyanoacrylate The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyano.. |
|||
Cure Time | >= 0.167 min | >= 0.00278 hour | Fixture |
Resinlab® CYNERGY CA6002 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.167 min | >= 0.00278 hour | Fixture |
Resinlab® CYNERGY CA6501 Adhesive Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Cure Time | >= 0.167 min | >= 0.00278 hour | Fixture |
Resinlab® CYNERGY CA6802 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | >= 0.167 min | >= 0.00278 hour | Fixture |
Resinlab® CYNERGY CA6806 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application .. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed
(disc Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength.Application areas: Moldings for higher mechanical strain, e.g. power plugs high volta.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage
(discontinued **)& Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak .. |
|||
Cure Time | <= 0.167 min | <= 0.00278 hour | |
Dymax 9-911 Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-911 Strain Relief, Wire and Parts Tacking AdhesiveRapid, high strength, designed for difficult substrates, resists.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Cooling Time |
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent
soft touch feel a.. |
|||
Cure Time | 0.167 - 0.250 min | 0.00278 - 0.00417 hour | ABS, handling time |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Cure Time | 0.167 - 0.250 min | 0.00278 - 0.00417 hour | Steel, handling time |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.Application areas: Thermally and dyna.. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled, elasticized. Very good heat resistance, very good mechanical properties, reduced mold shrinkage and post-shrinkage, good .. |
|||
Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte.. |