Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 40.0 - 60.0 min | 0.667 - 1.00 hour | working strength |
Permabond TA430 Acrylic Adhesive & Initiator PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | working strength |
Permabond TA435 Toughened Acrylic Adhesive & Initiator PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | working strength |
Permabond TA436 Toughened Acrylic Adhesive PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | Anaerobic cure speed |
Permabond UV7141 UV-curable Adhesive Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet.. |
|||
Cure Time | 3.00 - 60.0 min @Temperature 60.0 - 170 °C |
0.0500 - 1.00 hour @Temperature 140 - 338 °F |
Average value: 25.8 min Grade Count:12 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Cure Time | 10.0 - 60.0 min | 0.167 - 1.00 hour | Average value: 21.3 min Grade Count:6 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Cure Time | 10.0 - 60.0 min | 0.167 - 1.00 hour | Dry Time to Handling; Fed Std 141 4061 |
Humiseal 1C49 Silicone Conformal Coating Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
Cure Time | 15.0 - 60.0 min @Temperature 23.0 °C |
0.250 - 1.00 hour @Temperature 73.4 °F |
|
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Cure Time | 45.0 - 60.0 min @Temperature 60.0 °C |
0.750 - 1.00 hour @Temperature 140 °F |
Full cure in 45 to 60 mins at 140°F. |
Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive Description:#1101 is a light grayish-tan two part epoxy adhesive that was developed especially for difficult bonding problems involving similar or dissimilar materials. #1101 provides excellent adhe.. |
|||
Cure Time | 30.0 - 60.0 min @Temperature 150 °C |
0.500 - 1.00 hour @Temperature 302 °F |
|
Lord Adhesives 6100 Silver Conductor LORD 6100 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and di.. |
|||
Cure Time | 30.0 - 60.0 min @Temperature 125 °C |
0.500 - 1.00 hour @Temperature 257 °F |
|
Lord Adhesives Thermosetâ„¢ MS-330 Silicone Board Level Encapsulant LORD Thermosetâ„¢ MS-330 encapsulant is a one component silicone specifically designed for use on high-frequency devices including Bluetooth applications. This silicone encapsulant offers excelle.. |
|||
Cure Time | 45.0 - 60.0 min | 0.750 - 1.00 hour | Functional cure |
ITW Devcon 5 minute® Epoxy Gel, Opaque Information provided by ITW Devcon |
|||
Cure Time | 45.0 - 60.0 min | 0.750 - 1.00 hour | Functional cure |
ITW Devcon 5 minute® Epoxy, Light Amber Information provided by ITW Devcon |
|||
Cure Time | 45.0 - 60.0 min | 0.750 - 1.00 hour | Functional cure |
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black Information provided by ITW Devcon |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | |
Trelleborg Emerson & Cuming Stycast® 2057FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | |
Trelleborg Emerson & Cuming Stycast® 2850FT-FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | Dry to touch, RT @ 50%RH |
3M CP 25WB+ Fire Barrier Sealant 3M Fire Barrier Sealant CP 25WB+ is a high-performance, ready-to-use, gun-grade, latex-based, intumescent sealant that dries to form a monolithic fire-stop seal that also acts as a barrier to airbor.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | Dry to touch, RT @ 50%RH |
3M IC 15WB+ Fire Barrier Sealant 3M Fire Barrier Sealant IC 15WB+ is a cost-effective, one-part, gun-grade, latex-based, intumescent firestop sealant that dries to form a monolithic firestop seal that also acts as a barrier to airb.. |
|||
Cure Time | 45.0 - 60.0 min | 0.750 - 1.00 hour | Tack Free Time, catalyzed with QM CAT RED 3 |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Cure Time | 45.0 - 60.0 min | 0.750 - 1.00 hour | Tack Free Time, catalyzed with QM CAT RED 3 |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Cure Time | 20.0 - 60.0 min @Temperature 24.0 °C |
0.333 - 1.00 hour @Temperature 75.2 °F |
|
BCC Products BC 4544 Polyester Carvable Wood Filler This polyester resin base compound is easy to use, sets in minutes and can be sanded or carved almost immediately. Acts like wood yet exhibits no grain problems. BC4544 Wood Filler can be carved, sa.. |
|||
Cure Time | 30.0 - 60.0 min @Temperature 25.0 °C |
0.500 - 1.00 hour @Temperature 77.0 °F |
demold time |
BCC Products DP-11-90 Urethane Casting DP-11-90 is an unfilled, low viscosity, quick setting two component urethane system. An easy to use 1 to 1 mix ratio (Part A/Part B), DP-11-90 offers the user a 3 minute working time with parts demo.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | Air Set prior to curing |
Aremco Aremco-Seal™ 529 High Temperature Specialty Coatings Silicone Transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | at 200°F; 0.75-1 hr at 480°F |
Aremco Aremco-Seal™ 529 High Temperature Specialty Coatings Silicone Transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Cure Time | 50.0 - 60.0 min | 0.833 - 1.00 hour | Tack-Free, 50% RH |
3M 560 Polyurethane Adhesive Sealant 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | Dry to touch, RT @ 50%RH |
3M FD 150+ Fire Barrier Sealant 3M Fire Barrier Sealant FD 150+ is an economical, ready to use, gun-grade, elastomeric sealant that dries to from a monolithic flexible firestop seal. 3M Fire Barrier Sealant FD 150+ firestops joint.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | Air Set prior to curing |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | Dry to touch, RT @ 50%RH |
3M 1003 SL Fire Barrier Water Tight Sealants 3M Fire Barrier Water Tight Sealants 1000 NS and 1003 SL are ready-to-use, single component, neutral cure, silicone sealants that cure upon exposure to atmospheric humidity to form a flexible firest.. |
|||
Cure Time | 30.0 - 60.0 min @Temperature 90.0 °C |
0.500 - 1.00 hour @Temperature 194 °F |
|
Gwent Electronic Materials C2040226D4 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |