Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 45.0 - 45.0 min @Temperature 100 - 100 °C |
0.750 - 0.750 hour @Temperature 212 - 212 °F |
Average value: 45.0 min Grade Count:1 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Cure Time | 40.0 - 45.0 min | 0.667 - 0.750 hour | Fixture time |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive, Off-White Information provided by ITW Devcon |
|||
Cure Time | 30.0 - 45.0 min | 0.500 - 0.750 hour | Functional cure |
ITW Devcon One minuteâ„¢ Epoxy Gel, Amber Information provided by ITW Devcon |
|||
Cure Time | 5.00 - 45.0 min | 0.0833 - 0.750 hour | |
Taiwan PU Corporation UR50 Polyester Urethane Rubber UR50 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Cure Time | 5.00 - 45.0 min | 0.0833 - 0.750 hour | |
Taiwan PU Corporation UR60 Polyester Urethane Rubber UR60 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Cure Time | 5.00 - 45.0 min | 0.0833 - 0.750 hour | |
Taiwan PU Corporation UR70 Polyester Urethane Rubber UR70 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Cure Time | 5.00 - 45.0 min | 0.0833 - 0.750 hour | |
Taiwan PU Corporation UR80 Polyester Urethane Rubber UR80 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Cure Time | 5.00 - 45.0 min | 0.0833 - 0.750 hour | |
Taiwan PU Corporation UR90 Polyester Urethane Rubber UR90 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Cure Time | 30.0 - 45.0 min | 0.500 - 0.750 hour | Tack-free |
Sika Industry SikaFlex 252 One Part Polyurethane Adhesive Sika 252 SikaFlex One Part Polyurethane AdhesiveA high viscous, high strength adhesive, this product can replace rivets, screws, welds, and other mechanical fasteners. Seals and bonds in one step. 4.. |
|||
Cure Time | 30.0 - 45.0 min | 0.500 - 0.750 hour | Tack-free |
Sika Industry SikaFlex 255FC Fast Cure One Part Polyurethane Adhesive Sika 255FC SikaFlex Fast Cure One Part Polyurethane AdhesiveThis is a fast curing flexible high performance polyurethane adhesive for bonding glass to metal surfaces. Initial strength is derived fro.. |
|||
Cure Time | 30.0 - 45.0 min | 0.500 - 0.750 hour | At 160°F plus 2-3 hrs at 300°F |
Master Bond EP30-3 High Temperature Resistant Two Component Epoxy Master Bond Polymer System EP30-3 is a two component, low viscosity epoxy featuring optical clarity and high temperature serviceability up to 450°F along with superior chemical resistance. EP30-3 h.. |