Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10080 - 30240 min @Temperature 20.0 °C |
168.0 - 504.0 hour @Temperature 68.0 °F |
(1-3 weeks) |
Abatron AboCoat 8508-3 Self-Leveling Epoxy Coating and Resurfacer AboCoat 8508-3 is a self-leveling epoxy coating and resurfacer. It is used for heavy-duty protection and rebuilding of smooth, spalled, cracked, or pitted floors. It can be applied to concrete, maso.. |