Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10.0 - 30.0 min @Temperature -65.0 - 300 °C |
0.167 - 0.500 hour @Temperature -85.0 - 572 °F |
Handling |
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT TURBO SEAL SERIES 55 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature -65.0 - 300 °C |
0.167 - 0.500 hour @Temperature -85.0 - 572 °F |
Handling |
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT TURBO SEAL SERIES 65 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature -65.0 - 300 °C |
0.167 - 0.500 hour @Temperature -85.0 - 572 °F |
Handling |
Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT TURBO SEAL SERIES 75 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings with lubricating properties to facilitate proper assembl.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature -65.0 - 300 °C |
0.167 - 0.500 hour @Temperature -85.0 - 572 °F |
Handling |
Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT TURBO SEAL SERIES 80 is a high performance control strength anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings.NSF Certified Certified to ANSI/NSF Sta.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature -65.0 - 400 °C |
0.167 - 0.500 hour @Temperature -85.0 - 752 °F |
Handling |
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT TURBO SEAL SERIES 85 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The high lubricating properties of this compound preven.. |
|||
Cure Time | 10.0 - 30.0 min @Temperature -65.0 - 180 °C |
0.167 - 0.500 hour @Temperature -85.0 - 356 °F |
Handling |
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT TURBO SEAL SERIES 95 is a medium strength high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures rapidly in the absenc.. |
|||
Cure Time | 15.0 - 30.0 min | 0.250 - 0.500 hour | handling time |
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Cure Time | 15.0 - 30.0 min | 0.250 - 0.500 hour | handling time |
Permabond ET515 Epoxy Resin PERMABOND® ET515 is a 1:1 mixable epoxy adhesive. ET515 is a semi-flexible toughened adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Cure Time | 15.0 - 30.0 min | 0.250 - 0.500 hour | working strength |
Permabond TA4300 Toughened Acrylic Adhesive PERMABOND® TA4300 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Cure Time | 25.0 - 30.0 min | 0.417 - 0.500 hour | working strength |
Permabond TA4310 Toughened Acrylic Adhesive PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Cure Time | 25.00 - 30.0 min @Temperature -55.0 - 150 °C |
0.4167 - 0.500 hour @Temperature -67.0 - 302 °F |
Handling |
Palm Labs Adhesives TURBO-LOCK SERIES 17-OR Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-OR is a fast curing, GREEN, high strength, oil resistant, close fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly .. |
|||
Cure Time | 15.0 - 30.0 min | 0.250 - 0.500 hour | working strength |
Permabond TA4246 Toughened Acrylic Adhesive PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with .. |
|||
Cure Time | 15.0 - 30.0 min | 0.250 - 0.500 hour | working strength |
Permabond TA4302 Toughened Acrylic Adhesive PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Cure Time | 10.0 - 30.0 min | 0.167 - 0.500 hour | Dry Time to Handling; Fed Std 141 4061 |
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Cure Time | 10.0 - 30.0 min | 0.167 - 0.500 hour | Dry Time to Handling; Fed Std 141 4061 |
Humiseal 1C65 Silicone Conformal Coating Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Cure Time | 15.0 - 30.0 min | 0.250 - 0.500 hour | |
Lord Adhesives 360 Sag-Resistant, High-Performance, 5 min Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 15.0 - 30.0 min | 0.250 - 0.500 hour | Set to Touch |
Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. T.. |
|||
Cure Time | 18.0 - 30.0 min @Temperature 23.0 °C |
0.300 - 0.500 hour @Temperature 73.4 °F |
|
Master Bond EP65HT-1 Fast Curing High Glass Transition Temperature Epoxy System Master Bond Polymer System EP65HT-1 features the unusual combination of ultra-fast cures and high temperature resistance. While typical fast setting epoxies normally possess glass transition tempera.. |
|||
Cure Time | 25.0 - 30.0 min | 0.417 - 0.500 hour | Tack-Free, 50% RH |
3M 730 Clear Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
Cure Time | 10.0 - 30.0 min | 0.167 - 0.500 hour | Tack-Free, 50% RH |
3M 755FC Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
Cure Time | 20.0 - 30.0 min | 0.333 - 0.500 hour | |
BCC Products DP-11-75 Urethane Adhesive DP-11-75 is a two component medium viscosity urethane patch system. A hybrid product which was designed specifically for making quick responsive repairs/buildups to the MB 4000 Foundry Plank. DP-11-.. |
|||
Cure Time | 10.0 - 30.0 min | 0.167 - 0.500 hour | Tack-Free, 50% RH |
3M 760 Hybrid Adhesive Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |