Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Functional |
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT TURBO SEAL SERIES 65 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between.. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Functional |
Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT TURBO SEAL SERIES 75 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings with lubricating properties to facilitate proper assembl.. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Functional |
Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT TURBO SEAL SERIES 80 is a high performance control strength anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings.NSF Certified Certified to ANSI/NSF Sta.. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Functional |
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT TURBO SEAL SERIES 85 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The high lubricating properties of this compound preven.. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Functional |
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT TURBO SEAL SERIES 95 is a medium strength high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures rapidly in the absenc.. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Functional |
Palm Labs Adhesives TURBO-LOCK SERIES 17-OR Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-OR is a fast curing, GREEN, high strength, oil resistant, close fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly .. |
|||
Cure Time | 180 - 240 min | 3.00 - 4.00 hour | handling time |
Permabond ET538 Epoxy Resin PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia.. |
|||
Cure Time | 180 - 240 min | 3.00 - 4.00 hour | Handling strength in 3 to 4 hrs. |
Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive Description:#1101 is a light grayish-tan two part epoxy adhesive that was developed especially for difficult bonding problems involving similar or dissimilar materials. #1101 provides excellent adhe.. |
|||
Cure Time | 120 - 240 min @Temperature 25.0 °C |
2.00 - 4.00 hour @Temperature 77.0 °F |
Tack Free; 50% relative humidity |
Lord Adhesives Aeroglaze® Z3480 High Solids Aromatic Polyurethane Coating Aeroglaze® Z3480 coating is designed for use on properly prepared and primed metal surfaces, in regions requiring a VOC below 335.8 g/l (2.8 lbs/gallon).All information provided by Lord. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Functional cure |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Straw, Black Information provided by ITW Devcon |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Functional cure |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White Information provided by ITW Devcon |
|||
Cure Time | 180 - 240 min @Temperature 149 °C |
3.00 - 4.00 hour @Temperature 300 °F |
|
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive .. |
|||
Cure Time | 120 - 240 min @Temperature 23.0 °C |
2.00 - 4.00 hour @Temperature 73.4 °F |
|
Master Bond Mastersil 773 Fast Curing Low Viscosity Silicone Master Bond MasterSil 773 is a ready-to-use one component ultra-low viscosity silicone elastomer based conformal coating which provides excellent protection to electronic circuitry in high humidity .. |
|||
Cure Time | 120 - 240 min @Temperature 121 - 163 °C |
2.00 - 4.00 hour @Temperature 250 - 325 °F |
|
Master Bond Supreme 46HT-2 Toughened, High Shear and Peel Strength Adhesive Description: Master Bond Supreme 46HT-2 is a two component epoxy adhesive featuring an attractive balance of good shear and peel strengths for high performance structural bonding and coating suitabl.. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | |
Trelleborg Emerson & Cuming Stycast® 2072 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | |
Trelleborg Emerson & Cuming Stycast® E 1400 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Cure Time | 30.0 - 240 min | 0.500 - 4.00 hour | Full Cure; Primed |
Loctite® Gasket Eliminator® 518 Flange Sealant Anaerobic GasketingLoctite® 518 Flexible Cure Gasket Eliminator® Flange SealantForms a flexible, solvent-resistance seal that will not tear or decay. Seals to 300ºF and fills gaps to 0.050". Can.. |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Tack Free Time, catalyzed with Moldmaster Red |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Cure Time | 180 - 240 min | 3.00 - 4.00 hour | Touch Dry |
3M Scotchkote™ 162CR Epoxy Coating 3M Scotchkote Epoxy Coating 162CR has been specifically developed as a 100% solids lining for eth internals of tanks, vessels and other equipment in contact with dirty water, mild aqueous chemicals .. |
|||
Cure Time | 180 - 240 min | 3.00 - 4.00 hour | Touch Dry |
3M Scotchkote™ UV 840 Urethane Coating Scotchkote Urethane Coating UV 840 has been developed to provide a durable gloss finish for use as the final coat of 3M coating systems in the construction and transport industries, where an ease of.. |
|||
Cure Time | 210 - 240 min @Temperature 24.0 °C |
3.50 - 4.00 hour @Temperature 75.2 °F |
demold time |
BCC Products SLO-KAST BC 8009 Urethane Casting Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user lo.. |
|||
Cure Time | 180 - 240 min @Temperature 149 °C |
3.00 - 4.00 hour @Temperature 300 °F |
Alternate Cure |
Aremco Aremco-Bond™ 526N High Performance Epoxide Clear-Amber, 1:1 System for Tough Bonding Applications Also available filled with aluminum oxide (Alumina) or pigments |
|||
Cure Time | 120 - 240 min | 2.00 - 4.00 hour | Tack Free Time, catalyzed with Moldmaster Red |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Cure Time | 120 - 240 min @Temperature 25.0 °C |
2.00 - 4.00 hour @Temperature 77.0 °F |
demold time |
BCC Products BC 8405 Urethane Casting BC8405 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8405 will exhibit high impact strength and yield thermoplastic-like parts. Some features i.. |
|||
Cure Time | 60.0 - 240 min @Temperature 93.3 °C |
1.00 - 4.00 hour @Temperature 200 °F |
preceeded by 1 hour air set |
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Cure Time | 30.0 - 240 min | 0.500 - 4.00 hour | Full Cure; Primed |
Loctite® Gasket Eliminator® 504 Flange Sealant Anaerobic GasketingLoctite® 504 Gap Filling Rigid Cure Gasket Eliminator® Flange SealantA single-component, instant low pressure seal that fills gaps to 0.030". Typical Use: Gap filling |
|||
Cure Time | 180 - 240 min | 3.00 - 4.00 hour | At 300°F plus 1 hrs at 150°F |
Master Bond Supreme 45HTQ Quartz Filled, Heat Resistant Epoxy Compound Master Bond Polymer Adhesive Supreme 45HTQ is a two component, toughened, quartz filled epoxy compound for high performance structural bonding and casting. It is suitable for applications where long.. |
|||
Cure Time | 30.0 - 240 min | 0.500 - 4.00 hour | Full Cure; Primed |
Loctite® Gasket Eliminator® 510 Flange Sealant Anaerobic GasketingLoctite® 510 High Temperature Rigid Cure Gasket Eliminator® Flange SealantProduct has a temperature range to 400ºF with excellent solvent and chemical resistance. Makes or dre.. |