Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1.33 - 2.33 min | 0.0222 - 0.0389 hour | Gelation time |
Mitsui MILEX™ RN-2410MB Acrylic Rubber Modified Phenolic Resin
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |