Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | handling time |
Permabond TA4310 Toughened Acrylic Adhesive PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | fixture time |
Permabond TA4810 Toughened Acrylic Adhesive PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4810 has excellent adhesion to as received metal surfac.. |
|||
Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | Fixture time |
ITW Devcon 5 minute® Epoxy Gel, Opaque Information provided by ITW Devcon |
|||
Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | Fixture time |
ITW Devcon 5 minute® Epoxy, Light Amber Information provided by ITW Devcon |
|||
Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | Fixture time |
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black Information provided by ITW Devcon |
|||
Cure Time | 11.0 - 15.0 min | 0.183 - 0.250 hour | Fixture time |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive FC, Off-White, Black Information provided by ITW Devcon |
|||
Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | Fixture time |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive, Straw, White, Black Information provided by ITW Devcon |
|||
Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | Tack-free |
Sika Industry SikaTack UltraFast Fast Cure One Part Polyurethane Adhesive Sika UltraFast SikaTack Fast Cure One Part Polyurethane AdhesiveThis revolutionary product uses heat instead of moisture to "pre-cure" the adhesive. The product is heated before applications using a.. |
|||
Cure Time | 10.0 - 15.0 min | 0.167 - 0.250 hour | Tack-free time |
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of .. |
|||
Cure Time | 0.417 - 15.0 min | 0.00694 - 0.250 hour | Tack Free Time |
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria.. |