Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0194 hour | On Steel (Fixture) |
ND Industries 354 Surface Insensitive Instant Superglue Gel for porous, hard to bond surfaces - large gap |
|||
Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0194 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 309 Non-running gel for porous surfaces, general purpose |
|||
Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0195 hour | Dry Time |
Loctite® 7649 Acetone Base Primer N Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |
|||
Cure Time | 1.00 - 1.17 min | 0.0167 - 0.0194 hour | per mm |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Cure Time | 0.833 - 1.17 min | 0.0139 - 0.0194 hour | per mm |
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom.. |
|||
Cure Time | 0.333 - 1.17 min | 0.00555 - 0.0195 hour | Time to Handling Strength |
3M Scotch-Weld™ LO1000 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0195 hour | Dry Time |
Loctite® 7471 Acetone/Isopropanol Base Primer T Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |