Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | On Steel (Fixture) |
ND Industries 388 Toughened Instant Superglue Black toughened Cyanoacrylate for metal, rubber, and plastic |
|||
Cure Time | 0.583 - 1.00 min | 0.00972 - 0.0167 hour | On Steel (Fixture) |
ND Industries High Temperature SuperGlue 311 Very high viscosity with thermal cycling resistance |
|||
Cure Time | 0.417 - 1.00 min | 0.00694 - 0.0167 hour | On Steel (Fixture) |
ND Industries High Temperature SuperGlue 362 Medium viscosity with thermal cycling resistance |
|||
Cure Time | 0.417 - 1.00 min | 0.00694 - 0.0167 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 316 Medium-high viscosity for gap fillingMeets military spec Mil-A-46050C Type II Class III |
|||
Cure Time | 0.417 - 1.00 min | 0.00694 - 0.0167 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 322 High viscosity for large gap filling non-metallic surfacesMeets military spec Mil-A-46050C Type II Class III |
|||
Cure Time | 0.333 - 1.00 min | 0.00556 - 0.0167 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 344 Medium viscosity, general purposeMeets military spec Mil-A-46050C Type II Class III |
|||
Cure Time | 0.333 - 1.00 min | 0.00556 - 0.0167 hour | With Excel 600392 primer (Fixture) |
ND Industries 240 Structural Adhesive Excellent impact and solvent resistance |
|||
Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | Per 1 mm of wall thickness, compression molding |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
Cure Time | 0.833 - 1.00 min | 0.0139 - 0.0167 hour | per mm |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Cure Time | 0.250 - 1.00 min | 0.00417 - 0.0167 hour | |
3M Scotch-Weld™ CA5 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity, slower setting version of CA4 for filling gaps. Meets CID A-A-3097, Type II, Clas.. |
|||
Cure Time | 0.333 - 1.00 min | 0.00555 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ EC2500 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Cure Time | 0.167 - 1.00 min | 0.00278 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ LO100 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Cure Time | 0.0833 - 1.00 min | 0.00139 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ LO5 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Cure Time | 0.0833 - 1.00 min | 0.00139 - 0.0167 hour | Time to Handling |
3M Scotch-Weld™ MG05 LO Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.167 - 1.00 min | 0.00278 - 0.0167 hour | Time to Handling |
3M Scotch-Weld™ MG100 LO Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Product Introduction: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC t.. |
|||
Cure Time | 0.0833 - 1.00 min | 0.00139 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ EC600 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ PR Gel Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ SI Gel Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI Gel (formerly SB09) is a fas.. |
|||
Cure Time | 0.0833 - 1.00 min | 0.00139 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ SI1500 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI1500 is a surface insensitive.. |
|||
Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most .. |
|||
Cure Time | 0.500 - 1.00 min | 0.00833 - 0.0167 hour | Per 1 mm of wall thickness, compression molding |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |