Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 2160 - 2880 min | 36.0 - 48.0 hour | 90% of maximum strength developed within |
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or .. |
|||
Cure Time | 2160 min @Temperature 22.0 °C |
36.0 hour @Temperature 71.6 °F |
|
Dow Corning 748 NON-CORROSIVE SEALANT White, neutral cure RTV sealant especially for electrical applications.Information provided by Dow Corning |