Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cure Time = 11.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 11.0 min

@Temperature 155 °C
0.183 hour

@Temperature 311 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-759 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-326 (HS-HAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-990 (MT)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-326 (HS-HAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 160 °C
0.183 hour

@Temperature 320 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 11.0 min

@Temperature 68.3 °C
0.183 hour

@Temperature 155 °F
Press cured
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Cure Time 11.0 min

@Temperature 160 °C
0.183 hour

@Temperature 320 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 11.0 min

@Temperature 155 °C
0.183 hour

@Temperature 311 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-759 Plasticizer
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-326 (HS-HAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-774 (SRF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-990 (MT)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-326 (HS-HAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-774 (SRF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-990 (MT)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-990 (MT)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Oyster Shell Calcium Carbonate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 160 °C
0.183 hour

@Temperature 320 °F
Press cured
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.5 PHR Sulfur
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-774 (SRF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-326 (HS-HAF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-774 (SRF)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-990 (MT)
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Oyster Shell Calcium Carbonate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Translink 555
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 11.0 min

@Temperature 68.3 °C
0.183 hour

@Temperature 155 °F
Press cured
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..