Polymer Property : Cure Time = 0.267 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea
EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim..
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea
EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr..
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa..
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea
EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL..
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone
EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi..
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC EP RP EPI Engineered Polymers Aromatic Polyurea
EP RP, Aromatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RP displays extremely fast cure time..
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC EP RSP EPI Engineered Polymers Silicone Polyurea
EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time..
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer
EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti..
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea
ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst..