Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | >= 0.0500 min | >= 0.000833 hour | on metal (Fixture) |
ND Industries 623 Heptane-Acetone SuperGlue accelerator Fast Acting SuperGlue accelerator, general purpose for porous surfaces or large gaps. Non-ozone depleting but flammable solvent |
|||
Cure Time | 0.0500 - 0.0833 min | 0.000833 - 0.00139 hour | Steel, handling time |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Cure Time | 0.0500 - 0.0833 min | 0.000833 - 0.00139 hour | Buna N Rubber, set time |
Permabond 930 Cyanoacrylate PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The .. |
|||
Cure Time | 0.0500 - 0.0833 min | 0.000833 - 0.00139 hour | Rubber set time |
Lord Adhesives 6900 Medium Viscosity, Low Odor, Low Bloom Butyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0500 - 0.0667 min | 0.000833 - 0.00111 hour | Plastic set time |
Lord Adhesives 7000 Medium Setting, Medium Viscosity, Moisture Resistant Methyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | <= 0.0500 min | <= 0.000833 hour | Fixture Time, Glass side exposed to 10 mW/cm<sup>2</sup> @ 365 nm |
3M Scotch-Weld™ MG6500-74 UV/VIS Medical Grade Light Cure Adhesive 3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing .. |
|||
Cure Time | 0.0500 - 0.333 min | 0.000833 - 0.00555 hour | Time to Handling Strength |
3M Scotch-Weld™ PR40 Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Cure Time | 0.0500 - 0.333333 min | 0.000833 - 0.00555555 hour | |
3M Scotch-Weld™ CA40 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to many substrates including flexible vinyl and EPDM rubbe.. |
|||
Cure Time | 0.0500 - 0.500 min | 0.000833 - 0.00833 hour | Time to Handling |
3M Scotch-Weld™ MG100 SF Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.0500 - 0.500 min | 0.000833 - 0.00833 hour | Time to Handling |
3M Scotch-Weld™ MG20 SF Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.0500 - 0.500 min | 0.000833 - 0.00833 hour | Time to Handling Strength |
3M Scotch-Weld™ SF100 Super Fast Instant Adhesive 3M™ Scotch-Weld™ Super Fast Instant Adhesives rely less on surface moisture for cure speed than standard cyanoacrylates. They are designed to join together difficult-to-bond plastics and rubbers, .. |
|||
Cure Time | 0.0500 - 0.500 min | 0.000833 - 0.00833 hour | Time to Handling Strength |
3M Scotch-Weld™ SF20 Super Fast Instant Adhesive 3M™ Scotch-Weld™ Super Fast Instant Adhesives rely less on surface moisture for cure speed than standard cyanoacrylates. They are designed to join together difficult-to-bond plastics and rubbers, .. |
|||
Cure Time | 0.0500 - 0.333 min | 0.000833 - 0.00555 hour | Time to Handling Strength |
3M Scotch-Weld™ SI100 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI100 is a low viscosity produc.. |