Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2755C Thermoplastic Elastomer (TPE) Dynaflex™ G2755C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypropylene .. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® K4GA4070A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | Injection Molding |
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
LG Chemical Lupox® HI-2302 High Impact PBT, 30% Glass Fiber Reinforced LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Screw Speed | 50 - 75 rpm | 50 - 75 rpm | |
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Screw Speed | 50 - 75 rpm | 50 - 75 rpm | |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Screw Speed | 50 - 75 rpm | 50 - 75 rpm | |
MTI ThermoStran® PA66-30C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Screw Speed | 50 - 75 rpm | 50 - 75 rpm | |
MTI ThermoStran® PA66-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Screw Speed | 50 - 75 rpm | 50 - 75 rpm | |
MTI ThermoStran® TPU-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Screw Speed | 50 - 75 rpm | 50 - 75 rpm | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
Star Plastics PC1212FR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
Star Plastics PC701 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |