Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem AB870LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem GP-9401 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem GP-980 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 241-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | <= 100 rpm | <= 100 rpm | |
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin 15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Screw Speed | <= 100 rpm | <= 100 rpm | |
Beijing Chemical Industry KAIFA® 301-G10F PBT Resin 10% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Screw Speed | 100 rpm | 100 rpm | |
Beijing Chemical Industry KAIFA® GL6000 ABS Metal Plating Grade Excellent plating performance, Good thermal stabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | <= 100 rpm | <= 100 rpm | |
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance .. |