Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 50 - 70 rpm | 50 - 70 rpm | |
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
PTS Tristar® PC-10R-CL 10 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUCON PS4200 ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch.. |
|||
Screw Speed | 30 - 70 rpm | 30 - 70 rpm | Injection Molding |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LG Chemical LUPOY GP-5306F General Purpose PC/ABS Alloy, 30% Polymer Alloy, Weather Resistant, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUPOY SC1004A PC Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LTL Color Compounds ColorFast® NYA1000 Nylon/ABS Alloy Nylon/ABS alloy with high ductility and excellent chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled 30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUPOY ER5001RF PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (All in One PC & Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by .. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LG Chemical LUPOY GN-2006F Halogen Free Modified PC, Unreinforced, Weather Resistant, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUPOY GN2301F PC+GF30%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF30%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Screw Speed | 50 - 70 rpm | 50 - 70 rpm | |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
LG Chemical LUPOY SC1004ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LG Chemical LUPOY SR-3108F High Flow Modified PC, 10% Mineral Fillers, High Reflectivity, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc. |