Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 25 - 110 rpm | 25 - 110 rpm | |
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE) Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good .. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® K4GA4070A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® V2GA1065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2701C Thermoplastic Elastomer (TPE) Dynaflex™ G2701C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Rubbery Feel.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABS3030 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABS9020 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSLG5035 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Screw Speed | 25 - 80 rpm | 25 - 80 rpm | |
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose Data provided by Clariant Masterbatches |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® K2GA4055D TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |