Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 1020 C Polypropylene Calcium Carbonate Filler, 10% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 1505 R Polypropylene Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 24.9 - 50.0 psi | |
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® OBC 4755A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1123 BLK 111 Thermoplastic Elastomer Uses: General Purpose; Grommets; Weather Stripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 1.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1155B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1934C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-2318G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-2452L Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-2460B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-2555A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-2575F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-89-P834-B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1996E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-2365A Thermoplastic Polyolefin Elastomer Uses: Automotive Applications; Flexible Grips; Gaskets; General Purpose; Industrial Applications; Roof Vents Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injectio.. |
|||
Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
Clariant Renol PA211 Nylon 6, General Purpose Data provided by Clariant Masterbatches |
|||
Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
Clariant Renol PA211N40 Nylon 6, Mineral/Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |