Polymer Property : Back Pressure = 49.3 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.170 - 0.340 MPa
24.7 - 49.3 psi
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
Back Pressure 0.170 - 0.340 MPa
24.7 - 49.3 psi
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
Back Pressure 0.170 - 0.340 MPa
24.7 - 49.3 psi
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..