Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.0300 - 0.300 MPa | 4.35 - 43.5 psi | |
Huntsman AVALON® 60 ABX Thermoplastic Polyurethane Introduction: AVALON 60 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Back Pressure | 0.0300 - 0.300 MPa | 4.35 - 43.5 psi | |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax CCP PBT 1100-211X Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 4140-201D 40% Glass Fiber Filled Product Description: A glass fiber 40% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Back Pressure | 0.0300 - 0.300 MPa | 4.35 - 43.5 psi | |
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi.. |
|||
Back Pressure | 0.0300 - 0.300 MPa | 4.35 - 43.5 psi | |
Huntsman AVALON® 70 AE Thermoplastic Polyurethane Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Back Pressure | 0.0300 - 0.300 MPa | 4.35 - 43.5 psi | |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Back Pressure | 0.0300 - 0.300 MPa | 4.35 - 43.5 psi | |
Huntsman AVALON® 85 AE Thermoplastic Polyurethane Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Back Pressure | 0.0300 - 0.300 MPa | 4.35 - 43.5 psi | |
Huntsman AVALON® 90 AK Thermoplastic Polyurethane Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax CCP PBT 1100-600S Product Description: PBT unreinforced high viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excell.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 2000-104D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 2000-201D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 3030-104 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax CCP PBT 3010-104 10% Glass Fiber Filled Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 1100-211MB Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Back Pressure | 0.0300 - 0.300 MPa | 4.35 - 43.5 psi | |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |