Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | |
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Back Pressure | 0.400 - 1.00 MPa | 58.0 - 145 psi | |
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa JH720 G20 20% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa JH720 G30 30% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Back Pressure | 0.700 - 1.00 MPa | 102 - 145 psi | |
Kingfa JH830T Flame Retardant PC Features:UL V-0 @ 2.4mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceTransparentApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInfor.. |
|||
Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
Kingfa JH950-502 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesGood low temperature resistanceGood normal/low temperature impact strengthGood surfaceApplications:ControllerPlugSocketShell of ammeterInformation .. |
|||
Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa MAC-751 PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem AB870LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem GP-975B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem MP-855WR TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer Zythane™ 4060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.499 - 1.00 MPa | 72.4 - 145 psi | Injection |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.499 - 1.00 MPa | 72.4 - 145 psi | Injection |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.200 - 1.00 MPa | 29.0 - 145 psi | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly.. |
|||
Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)
(discontinu The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |