Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.517 - 1.21 MPa | 75.0 - 175 psi | |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Back Pressure | 0.517 - 0.862 MPa | 75.0 - 125 psi | |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Back Pressure | 0.517 - 1.21 MPa | 75.0 - 175 psi | |
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s.. |
|||
Back Pressure | 0.517 - 1.21 MPa | 75.0 - 175 psi | |
Elastocon TPE Technologies Elastocon® STK60B Thermoplastic Elastomer Elastocon® STK60B black thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60B is well suited for .. |
|||
Back Pressure | 0.517 - 1.21 MPa | 75.0 - 175 psi | |
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer.. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S310 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S319 Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S519 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S610 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S710 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA T-120 Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA TW-18B2 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA TW-20 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA/PC TA-35 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 MPa | 75.0 psi | |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Back Pressure | 0.517 - 1.21 MPa | 75.0 - 175 psi | |
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s.. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA M-143 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |