Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | <= 15.0 MPa | <= 2180 psi | Specific |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Back Pressure | <= 15.0 MPa | <= 2180 psi | Specific |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |
|||
Back Pressure | <= 15.0 MPa | <= 2180 psi | Specific |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Back Pressure | <= 15.0 MPa | <= 2180 psi | Specific |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Back Pressure | <= 15.0 MPa | <= 2180 psi | Specific |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |
|||
Back Pressure | <= 15.0 MPa | <= 2180 psi | Specific |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Back Pressure | <= 15.0 MPa | <= 2180 psi | Specific |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v.. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia.. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |
|||
Back Pressure | 15.0 - 20.0 MPa | 2180 - 2900 psi | Molding Pressure |
Azoty Tarnow™ TARFLEN SM-1 PTFE Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |