Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.689 - 1.38 MPa | 99.9 - 200 psi | |
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 99.9 - 200 psi | |
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE) Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p.. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10R-CL 10 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Star Plastics PC721HFR Molding Grade PC High Flow with Release Information provided by Star Plastics, Inc. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Star Plastics PC731 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Star Plastics PC733R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Samyang Trirex® PC-3020U 22 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons.. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Clariant Renol 6004G23 Nylon 6, 23% Glass Fiber Reinforced Data provided by Clariant Masterbatches |