Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products GC10P200-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural Applications: Component housingsStorage binsRecreational vehicle trim and bumpersInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products GC20P200-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsBoat handlesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T20P105-00FA 20% Talc Reinforced Polypropylene, FDA Compliant Components, Natural Applications: Food traysFood service implementsContainersConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.000 - 1.03 MPa | 0.000 - 149 psi | |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products G30P100-00 30% Glass Fiber Reinforced Polypropylene, Natural Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP531-679UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, 2B5A Black Ink Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.000 - 1.03 MPa | 0.000 - 149 psi | |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
CTC X-PRO CTC PP 2015 Polypropylene Impact Copolymer X-PRO PP 2015 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
CTC X-PRO PP 2021 Polypropylene Impact Copolymer X-PRO PP 2021 is an impact, polypropylene copolymer. It has general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |