Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE) Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE) Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 .. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Ovation Polymers Nemcon™ H ABS DP116P ABS ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Dynalloy™ OBC8000-T05 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where excepti.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S195A Thermoplastic Polyurethane Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S198A Thermoplastic Polyurethane Type: Estane® S198A is a Shore 98A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S360D Thermoplastic Polyurethane Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S368D Thermoplastic Polyurethane Type: Estane® S368D is a Shore 68D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S385A Thermoplastic Polyurethane Type: Estane® S385A is a Shore 85A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S395A Thermoplastic Polyurethane Type: Estane® S395A is a Shore 95A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availa.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S398A Thermoplastic Polyurethane Type: Estane® S398A is a Shore 98A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® T365A Thermoplastic Polyurethane Type: Estane® T365A is a Shore 70A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® T370A Thermoplastic Polyurethane Type: Estane® T370A is a Shore 74A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® T470A Thermoplastic Polyurethane Type: Estane® T470A is a Shore 77A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S175A Thermoplastic Polyurethane Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® S375D Thermoplastic Polyurethane Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Back Pressure | 0.207 - 0.552 MPa | 30.0 - 80.0 psi | |
Lubrizol Estane® T865A Thermoplastic Polyurethane Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation |