Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 3.00 - 17.0 MPa | 435 - 2470 psi | |
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Conditioned (2.5% Moisture) Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro.. |