Polymer Property : Back Pressure = 2.07 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Back Pressure >= 2.07 MPa
>= 300 psi
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..