Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.170 - 0.340 MPa | 24.7 - 49.3 psi | |
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Back Pressure | 0.170 - 0.340 MPa | 24.7 - 49.3 psi | |
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Back Pressure | 0.170 - 0.340 MPa | 24.7 - 49.3 psi | |
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |