Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 1020 C Polypropylene Calcium Carbonate Filler, 10% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 1505 R Polypropylene Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 2006 T Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 4012 X Platinum Polypropylene Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 4518 CUW Polypropylene Calcium Carbonate Filler, 45% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 5014 CUW Polypropylene Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N2000NHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N2015L Nylon 6 (Cond) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N2017THL Nylon 6 (DAM) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (Cond) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (Cond) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Multibase Multi-Pro® 2003 TI Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (DAM) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Solvay Technyl® C216V15 15% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Solvay Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Back Pressure | 0.138 - 0.345 MPa | 20.0 - 50.0 psi | |
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |