Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2 - 4 hour | 2 - 4 hour | No venting in an air circulating oven |
Polimeri Europa Sinkral® B 432/E ABS Resin Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPC GF2007 PD1 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPC GK8020 Polypropylene Copolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Asahi Kasei Tenac® 5012 Acetal Homopolymer
(discontinued **) Standard-flow grade, with reduced stiffness and increased elongation through addition of special polymers.Applications: Clips, fasteners, press-fit parts.This product is not a part of the standard p.. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | nominal; maximum drying time of 8 hours |
LTL Color Compounds ColorFast® PBA1000 PBT/ABS Alloy PBT/ABS alloy with excellent physical properties and chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV R.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Injection Molding |
Styrolution Luran® S 797 SE ASA Luran S 797 SE is an extrusion ASA grade with especially high notched impact strength, used for sheet and profile extrusions. The data representable is based on extruded sheet.Information provided .. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Option 3 |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | Predrying Time |
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Opened bags and gaylord boxes |
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman VOLOY™ 461 Glass Reinforced, Flame Retardant PBT Alloy Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Option 3 |
UBE UBESTA® 3030U Nylon 12 (After Hexane for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 2 - 4 hour @Temperature 79.4 °C |
2 - 4 hour @Temperature 175 °F |
to avoid degradation of mechanical properties |
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour @Temperature 79.4 °C |
2 - 4 hour @Temperature 175 °F |
to ensure moisture level is less than 0.10% |
Clariant Renol PPSP0017 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour @Temperature 71.1 °C |
2 - 4 hour @Temperature 160 °F |
to avoid surface defects |
Clariant Renol PPT20BN-346 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPC GF5020 Polypropylene Copolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPH TS15030 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | nominal; maximum drying time of 48 hours |
LTL Color Compounds ColorFast® FRPC400 Polycarbonate, Flame-Retarded Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | nominal; maximum drying time of 8 hours |
LTL Color Compounds ColorFast® NY2 Nylon 66 Nylon 6,6 with or without lubeAll information provided by LTL Color Compounders, Inc. |