Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
Unitika AXG-1500-300 Conditioned Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika P-5001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
Unitika U-8400H U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |
|||
Dry Time | 8.00 - 24.0 hour | 8.00 - 24.0 hour | |
Unitika FUN-8000 Characteristics: High impact strength High chemical resistance Transparency as high as polycarbonateInformation provided by Unitika Ltd. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Dry Time | 2 - 24.0 hour | 2 - 24.0 hour | |
Chi Mei Polylac® PA-747 ABS High impact |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 4.00 - 24.0 hour | 4.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod.. |
|||
Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
Unitika U-8000 U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |