Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 3.00 - 12.0 hour | 3.00 - 12.0 hour | |
Oxford Polymers PBT 30GF PBT, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and LubricantsSpecial Characteris.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Oxford Polymers PC 714-FR Series PC, Flame retardant Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Dry Time | 3.00 hour | 3.00 hour | |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Dry Time | 3.00 hour | 3.00 hour | |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Extrusion Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Dry Time | 3.00 - 6.00 hour | 3.00 - 6.00 hour | Injection Molding |
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical LUPOL TE5109 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Dry Time | 3.00 hour @Temperature 100 °C |
3.00 hour @Temperature 212 °F |
|
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Dry Time | 3.00 hour @Temperature 100 °C |
3.00 hour @Temperature 212 °F |
|
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Dry Time | 3.00 hour @Temperature 100 °C |
3.00 hour @Temperature 212 °F |
|
Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar.. |
|||
Dry Time | 3.00 hour @Temperature 80.0 °C |
3.00 hour @Temperature 176 °F |
|
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil.. |
|||
Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
LG Chemical LUPOY GP1000MU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection and Extrusion Molding |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Dry Time | 3.00 - 6.00 hour | 3.00 - 6.00 hour | |
Eurotec® Tecoform® PO20 NL RT POM, PTFE modified, natural Information provided by Eurotec® |
|||
Dry Time | 3.00 hour | 3.00 hour | Extrusion |
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Dry Time | 3.00 hour | 3.00 hour | Extrusion |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |