Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 4 - 6 hour | 4 - 6 hour | |
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding General purpose grade with better flowability than IH 830 but slightly below in heat resistanceMechanical strength and surface hardnessFeatures: Excellent transparency and eleganceWeather resistance.. |
|||
Dry Time | 3 - 6 hour | 3 - 6 hour | |
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Dry Time | 2 - 6 hour | 2 - 6 hour | |
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Dry Time | 2 - 6 hour | 2 - 6 hour | |
Lanxess Durethan® BKV 50 H2.0 EF DUS30 901510 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | |
LG Chemical LUPOY GN-5001TF Halogen Free PC/ABS Alloy, High Flow, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Dry Time | 2 - 6 hour | 2 - 6 hour | |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Dry Time | 2 - 6 hour | 2 - 6 hour | |
Lanxess Durethan® BKV 40H2.0 EF 900116 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Dry Time | 2 - 6 hour | 2 - 6 hour | |
Lanxess Durethan® C 38 FAM 000000 Copolyamide PA 6-Copolymer, non-reinforced, extrusionInformation provided by LANXESS. |
|||
Dry Time | 2 - 6 hour | 2 - 6 hour | |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | |
Samyang Tribit® 1500G30 Polybutylene Terephthalate, 30% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Oil (ASTM D471 No. 1) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | Option 2 |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | |
Asia International Enterprise (Hong Kong) 60G2-13GF Nylon 66, 13% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | |
Asia International Enterprise (Hong Kong) 60G3F Nylon 66, 15% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | Option 2 |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | |
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | Option 2 |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |