Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPH TS15010 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPH TS15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
Polykemi AB POLYfill PPH T20020 UV Polypropylene Homopolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
LG Chemical HI-151 ABS, Middle Impact Information Provided by LG Chem |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | nominal; maximum drying time of 12 hours |
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded 13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Styron EMERGEâ„¢ 4731-8 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Opened bags and gaylord boxes |
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Opened bags and gaylord boxes |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Dry Time | 2 - 4 hour @Temperature 71.1 °C |
2 - 4 hour @Temperature 160 °F |
to ensure moisture content is less than 0.2% |
Clariant Renol 6601FR Nylon 66, Flame Retardant Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour @Temperature 104 °C |
2 - 4 hour @Temperature 220 °F |
to ensure moisture level is less than 0.02% |
Clariant Renol TPU2087AFR Polyurethane Elastomer, Flame Retardant Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour @Temperature 79.4 °C |
2 - 4 hour @Temperature 175 °F |
to ensure moisture content is less than 0.2% |
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Dry) Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the.. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPH T5060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
Polykemi AB POLYfill PPHC EP1001F Polypropylene Information provided by Polykemi AB |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | Predrying |
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66 Information provided by A. Schulman. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Asahi Kasei Xyron® 220V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Dry Time | 2 - 4 hour | 2 - 4 hour | nominal; maximum drying time of 8 hours |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |