Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 8 - 12 hour | 8 - 12 hour | Demold time, catalyzed with Stretch Effect B |
ACC Stretch Effect QSI Quantum Silicones Stretch Effect 22 Durometer Addition Cure Translucent Moldmaking Material
& Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, fast demold time, high elongation, excellent flexibility. Applications: special effects, skin replicat.. |
|||
Dry Time | 8 - 12 hour | 8 - 12 hour | Demold time, catalyzed with QM 270B |
ACC QM 270 QSI Quantum Silicones 70 Durometer Addition Cure Moldmaking Material QM 270 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina Fine grain castable for potting and producing small tools. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 576-N High Temperature Potting & Casting Alumina Medium grain castable ceramic for large high temperature potting and tooling. Aremco offers a range of ceramic-based materials used for the assembly of high temperature, high power electrical devic.. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 645-N High Temperature Potting & Casting Material Silica Castable ceramic with low thermal conductivity. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina Fine grain castable ceramic. |
|||
Dry Time | >= 8 hour | >= 8 hour | Air dry |
Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate High Density, high strength molding compound. |
|||
Dry Time | 8 - 12 hour | 8 - 12 hour | Hard |
Abatron MasterMold 12-3 Flexible Mold Making Compound Master mold 12-3 is formulated for versatility, high elasticity and strength. It is a 2-component polyurethane system and can be easily spread on any model to produce a smooth bubble-free mold surf.. |
|||
Dry Time | 8 hour | 8 hour | |
BASF Ultramid® Seal-Fit PA6/66 (Conditioned) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |