Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 4 hour | 4 hour | |
Plastcom SLOVALEN PC 63 T 15-1M PP, 15% mineral filling FeaturesModified PP copolymer for injection moulding with the content of 15 % mineral filler, uv stabilized, good scratch resistance, low odor and very good flowability with good dimensional stabili.. |
|||
Dry Time | 4 hour | 4 hour | |
Plastcom SLOVALEN PQ 91T 5 PP, 5% mineral filling FeaturesModified PP for injection moulding with the content of 5 % mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Dry Time | 4 hour | 4 hour | |
Plastcom SLOVAMID 6 GF 30 FRG 4 LW PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Dry Time | 4 hour | 4 hour | |
Plastcom SLOVAMID 66/6 HI/1 PA66/6, improved strength FeaturesMix of polyamide 66/6 modified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets fo.. |
|||
Dry Time | 4 hour | 4 hour | |
Nilit Polynil® N66-P300 High Viscosity Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 4 hour | 4 hour | |
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 4 hour | 4 hour | |
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Dry Time | 4 hour | 4 hour | |
LNP Thermocomp® OF-1006 Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Dry Time | 4 hour | 4 hour | |
Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | to moisture < 0.01% |
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Dry Time | 4 hour | 4 hour | |
MTI ThermoStran® PA66-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | Option 2 |
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Dry Time | 4 hour | 4 hour | |
Ecomass® 1007TU78 Tungsten Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Polymers |
|||
Dry Time | 4 hour | 4 hour | |
Ecomass® 1080TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Dry Time | 4 - 6 hour | 4 - 6 hour | |
Asia International Enterprise (Hong Kong) 60G6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Dry Time | 4 hour | 4 hour | |
Beijing Chemical Industry KAIFA® MN201-G35 Nylon 66 Resin 35% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |