Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE) OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor.. |
|||
Dry Time | 1.00 hour | 1.00 hour | |
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |