Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
PTS PBT-20GFR 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC. |
|||
Drying Temperature | 100 - 140 °C | 212 - 284 °F | Injection Molding |
DuPont Performance Polymers Crastin® CE15315 BK010 PBT
(Unverified Data**) Crastin® CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Drying Temperature | 120 - 140 °C @Time 14400 - 21600 sec |
248 - 284 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PBT-RG152 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesHigh glossyGood surfaceNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInformation Provided by Kingfa S.. |
|||
Drying Temperature | 120 - 140 °C @Time 14400 - 21600 sec |
248 - 284 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PBT-RG30 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Drying Temperature | 120 - 140 °C @Time 14400 - 21600 sec |
248 - 284 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa PBT-RG002 Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Drying Temperature | 120 - 140 °C @Time 10800 - 18000 sec |
248 - 284 °F @Time 3.00 - 5.00 hour |
Pre-dry |
Kingfa PET-G15 15% Glass Fiber Reinforced PET Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Drying Temperature | 120 - 140 °C @Time 10800 - 18000 sec |
248 - 284 °F @Time 3.00 - 5.00 hour |
Pre-dry |
Kingfa PET-G30 30% Glass Fiber Reinforced PET Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT70 GR15 NL100 MB PET, 15% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Asia International Enterprise (Hong Kong) 30G3 Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Drying Temperature | 116 - 140 °C | 240 - 284 °F | Average value: 127 °C Grade Count:13 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Drying Temperature | 130 - 140 °C | 266 - 284 °F | Temperature can be reduced when using vacuum ovens. |
LATI LARTON K/30 30% Carbon Fiber Reinforced Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |