Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Drying Temperature | 80.0 - 120 °C | 176 - 248 °F | |
PolyOne Bergadur™ PB40 G15 blue Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Drying Temperature | 110 - 120 °C | 230 - 248 °F | |
PolyOne Bergadur™ PB400 G15 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Drying Temperature | 110 - 120 °C @Time 14400 - 21600 sec |
230 - 248 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect.. |
|||
Drying Temperature | 110 - 120 °C @Time 10800 - 14400 sec |
230 - 248 °F @Time 3.00 - 4.00 hour |
Pre-dry |
Kingfa JH720 G30 30% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical Lupox® SV1120M PBT Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C @Time 10800 sec |
212 - 248 °F @Time 3.00 hour |
|
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Drying Temperature | 90.0 - 120 °C | 194 - 248 °F | Predrying Temperature |
Tisan TISARBON® Flame Retardant (V0) Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Drying Temperature | 110 - 120 °C | 230 - 248 °F | Predrying Temperature |
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
Eurotec® Tecoform® PO20 AR10 NL HS POM, 10% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 80.0 - 120 °C | 176 - 248 °F | |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Drying Temperature | 90.0 - 120 °C | 194 - 248 °F | Pre-drying Temperature |
Asahi Kasei Xyron® X0722 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Drying Temperature | 80.0 - 120 °C | 176 - 248 °F | |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Drying Temperature | 100 - 120 °C @Time 10800 sec |
212 - 248 °F @Time 3.00 hour |
|
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri.. |
|||
Drying Temperature | 80.0 - 120 °C | 176 - 248 °F | |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Drying Temperature | 80.0 - 120 °C | 176 - 248 °F | |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |