Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 82.2 - 92.2 °C | 180 - 198 °F | |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 82.2 - 92.2 °C | 180 - 198 °F | |
Diamond Polymers ASA M-143 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |