Processing Properties Metric English Comments
Drying Temperature 166 - 177 °C

@Time 14400 sec
331 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7535 Polyphenylsulfone (PPSU)
Radel® R-7535 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu..
Drying Temperature 166 - 177 °C

@Time 14400 sec
331 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU)
Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu..
Drying Temperature 166 - 177 °C

@Time 14400 sec
331 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU)
Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product ..