Processing Properties Metric English Comments
Drying Temperature 79.4 °C
175 °F
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Drying Temperature 79.4 °C
175 °F
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6
Information provided by A. Schulman.
Drying Temperature 79.4 °C
175 °F
Opened bags and gaylord boxes
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Drying Temperature 79.4 °C
175 °F
A. Schulman Aqualoy® 645 Glass Fiber Reinforced Hydrolysis Resistant Nylon 66
Information provided by A. Schulman.
Drying Temperature 79.4 °C
175 °F
A. Schulman Aqualoy® 645 Glass Fiber Reinforced Hydrolysis Resistant Nylon 66
Information provided by A. Schulman.