Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 60.0 - 93.3 °C | 140 - 200 °F | Average value: 81.0 °C Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
PTS Trilac® FR1 ABS- Flame Retardant ABS Resin
(Unverified Data**) Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABS3030 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABS5035 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABS9020 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABSHFL Molding Grade ABS High Flow Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | 2 to 24 hrs; Dehumidifying Dryer |
Shuman 730 Utility White ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABS448T Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 87.8 - 93.3 °C | 190 - 200 °F | |
TPI Porene® ABS-KU650 Super High Heat ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-001 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-026 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-028 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-051 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-072 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-085 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-091 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-214 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-190 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-251 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |