Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Nilit Nilamid A3 H ZB High Impact PA66 Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas .. |
|||
Drying Temperature | 79.4 - 85.0 °C | 175 - 185 °F | |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Drying Temperature | 80.0 - 85.0 °C @Time 7200 - 10800 sec |
176 - 185 °F @Time 2.00 - 3.00 hour |
|
IRPC Polimaxx Polene GP150 Polystyrene APPLICATIONS: INJECTION MOULDING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARE, etc. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
Drying Temperature | 82.0 - 85.0 °C | 180 - 185 °F | |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ABS 3500ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ABS 3501 GF-30 Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ABS 7602B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers TR 5000 AS/P Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide A40 PA66, Extrusion Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide AG8 PA66, 40% Glass Fiber Reinforced, Injection Molding Staramide AG8 is a 40% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide PF005 PA6, 25% Glass Fiber Filled, Injection Molded Staramide PF005 is an 25% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide RF003S PA66, 15% Glass Fiber Filled, Injection Molded Staramide RF003S is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide RF004XXC PA6, 20% Glass Fiber Filled, Injection Molded Staramide RF004XXC is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide RF005S PA66, 25% Glass Fiber, Injection Molded Starflam RF005S is a 25% Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide RF007S PA66, 35% Glass Fiber Filled, Injection Molded Staramide RF007S is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ABS VP-11 Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |