Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 95.0 - 150 °C | 203 - 302 °F | Average value: 106 °C Grade Count:7 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Drying Temperature | 120 - 150 °C | 248 - 302 °F | Average value: 143 °C Grade Count:41 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Drying Temperature | 149 - 150 °C | 300 - 302 °F | Average value: 150 °C Grade Count:9 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Drying Temperature | 120 - 150 °C | 248 - 302 °F | Average value: 145 °C Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Drying Temperature | 121 - 150 °C | 250 - 302 °F | Average value: 140 °C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Drying Temperature | 121 - 150 °C | 250 - 302 °F | Average value: 142 °C Grade Count:30 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Drying Temperature | 50.0 - 150 °C | 122 - 302 °F | Average value: 130 °C Grade Count:14 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Drying Temperature | 50.0 - 150 °C | 122 - 302 °F | Average value: 122 °C Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latilub 80-10T K/15 PPS, 15% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latiohm 80-04 PD01 G/30 PPS, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Drying Temperature | 120 - 150 °C @Time 14400 sec |
248 - 302 °F @Time 4.00 hour |
|
Eurostar Starglas GX061104 PSU Starglas GX061104 is a PSU resin (also known as Starglas PSU A ¾)Information provided by Eurostar. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Laticonther 80 GR/50 PPS, 50% Graphite Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |