Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Drying Temperature | 110 - 120 °C | 230 - 248 °F | |
PolyOne Bergadur™ PB400 G15 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Drying Temperature | 110 - 120 °C | 230 - 248 °F | |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Drying Temperature | 110 - 120 °C | 230 - 248 °F | |
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT
(Unverified Data**) Crastin® LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has excellent surface aspect, dimensional stability and low warpage and was developed fo.. |
|||
Drying Temperature | 110 - 120 °C @Time 14400 - 21600 sec |
230 - 248 °F @Time 4.00 - 6.00 hour |
Pre-dry |
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect.. |
|||
Drying Temperature | 110 - 120 °C @Time 10800 - 14400 sec |
230 - 248 °F @Time 3.00 - 4.00 hour |
Pre-dry |
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne.. |
|||
Drying Temperature | 110 - 120 °C @Time 10800 - 14400 sec |
230 - 248 °F @Time 3.00 - 4.00 hour |
Pre-dry |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical Lupox® DP1000DU PBT Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
LG Chemical LUPOY GN2301F PC+GF30%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF30%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Drying Temperature | 100 - 120 °C @Time 10800 sec |
212 - 248 °F @Time 3.00 hour |
|
LATI Latilub 75/4-20T PBT, PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Drying Temperature | 110 - 120 °C | 230 - 248 °F | Predrying Temperature |
Tisan TISESTER® UNR Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
Eurotec® Tecoform® PO20 GR25 NL HS POM, 25% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 100 - 120 °C | 212 - 248 °F | |
Eurotec® Tecoform® PO30 GB20 NL HS POM, 20% glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 80.0 - 120 °C | 176 - 248 °F | |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Drying Temperature | 80.0 - 120 °C | 176 - 248 °F | |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |